A fire-rated MgO SIP wall panel is a sandwich panel with two magnesium oxide (MgO) board facings around a foam core, where the whole wall has been tested to a fire test standard and holds a rating such as 1 hour. The board is fire-resistant. The wall is fire-rated. These are two different claims.

What decides the rating
Three things, in this order:
- Facing thickness. 6 mm MgO gives less time than 12 mm. 10–12 mm is the usual choice for a 1-hour wall.
- Core type. EPS and XPS are combustible. A mineral wool core makes the panel non-combustible, which is what high-rise projects usually need.
- Joint detail. Most failures happen at the joint between panels. Use the spline or cam-lock system named in the test report, not a site invention.
The two tests people mix up
| Test | What it checks | What you get |
|---|---|---|
| ASTM E84 | Surface of one board | Class A, flame spread 0, smoke 5 |
| ASTM E119 | A full wall in a furnace | 1-hour or 2-hour rating |
E84 is cheap and looks good on a datasheet. E119 is what the building official asks for. Always ask which one the supplier means.
Where these walls are used
- Fire walls between modules in modular and prefab buildings
- Party walls and corridor walls in apartments, hotels, workforce housing
- Mezzanine separation in commercial fit-outs
- Cold storage and food plants
- Exterior walls of mid-rise buildings, where a separate exterior fire test (NFPA 285) may also apply